поискавой системы для электроныых деталей
  Russian  ▼
ALLDATASHEETRU.COM

X  

MMA200 датащи(PDF) 21 Page - Clarke International

номер детали MMA200
подробное описание детали  MMA/TIG INVERTER WELDERS
PDF  32 Pages
Scroll/Zoom Zoom In 100%  Zoom Out
производитель  CLARKE [Clarke International]
домашняя страница  https://www.clarkeinternational.com/
Logo CLARKE - Clarke International

MMA200 датащи(HTML) 21 Page - Clarke International

Back Button MMA200 Datasheet HTML 17Page - Clarke International MMA200 Datasheet HTML 18Page - Clarke International MMA200 Datasheet HTML 19Page - Clarke International MMA200 Datasheet HTML 20Page - Clarke International MMA200 Datasheet HTML 21Page - Clarke International MMA200 Datasheet HTML 22Page - Clarke International MMA200 Datasheet HTML 23Page - Clarke International MMA200 Datasheet HTML 24Page - Clarke International MMA200 Datasheet HTML 25Page - Clarke International Next Button
Zoom Inzoom in Zoom Outzoom out
 21 / 32 page
background image
21
Parts & Service: 020 8988 7400 / E-mail: Parts@clarkeinternational.com or Service@clarkeinternational.com
7. Switch ON using the switch mounted on the rear panel. The green light on
the front panel will glow.
8. If the machine stops at any time and the amber light comes ON, the
thermal overload has intervened. Wait until the welder has cooled
sufficiently (the amber light goes out) before restarting work. Open the gas
valve on the torch handle,
• This will allow gas to flow from the torch nozzle.
9. Cover your face with the head shield, bring the torch to within 3-4mm of
the work, and at an angle of 45°, so that the ceramic nozzle gently touches
the work surface.
10. Scratch the tip of the electrode against the piece to be welded, as soon as
the welding arc starts, remove the electrode to a distance of 3-4 mm, and
continue the weld. (See notes below).
• This method is referred to as ‘Scratch Arc’.
11. To stop welding, simply remove the torch from the workpiece.
12. Turn OFF the gas as soon as you finish welding.
Note:
• To avoid a visible strike mark on the surface of the workpiece it is
advisable to strike the arc in the joint where the mark will be
concealed by the weld.
• Thin sheet and stainless steel may be welded with or without filler,
similar to gas welding.
• The filler is fed in at the edge of the pool. The rod must not touch the
tip of the electrode or enter the arc. The end of the rod must always
be shielded by the argon atmosphere to prevent as far as possible
the formation of oxides of its surface. When welding stainless steel
and copper, it is often possible to feed in the filler continuously at the
edge of the pool.



Html Pages

1 2 3 4 5 6 7 8 9 10 11 12 13 14 15 16 17 18 19 20 21 22 23 24 25 26 27 28 29 30 31 32


датащи скачать

Go To PDF Page


ссылки URL



Вашему бизинису помогли Аллдатащит?  [ DONATE ] 

Что такое Аллдатащит   |   реклама   |   контакт   |   Конфиденциальность   |   Ссылка на техническое описание    |   обмен ссыками   |   поиск по производителю
All Rights Reserved©Alldatasheet.com


Mirror Sites
English : Alldatasheet.com  |   English : Alldatasheet.net  |   Chinese : Alldatasheetcn.com  |   German : Alldatasheetde.com  |   Japanese : Alldatasheet.jp
Russian : Alldatasheetru.com  |   Korean : Alldatasheet.co.kr  |   Spanish : Alldatasheet.es  |   French : Alldatasheet.fr  |   Italian : Alldatasheetit.com
Portuguese : Alldatasheetpt.com  |   Polish : Alldatasheet.pl  |   Vietnamese : Alldatasheet.vn
Indian : Alldatasheet.in  |   Mexican : Alldatasheet.com.mx  |   British : Alldatasheet.co.uk  |   New Zealand : Alldatasheet.co.nz
Family Site : ic2ic.com  |   icmetro.com